Mechanical Properties of Cold-Rolled Stainless Steel
Grades and Mechanical Properties
Grade | Mechanical Property | |||||||
Classification | NAS | JIS | Yield Strength |
Tensile Strength |
Elongation | Hardness | ||
(N/mm2) | (N/mm2) | (%) | (HRB) | (HV) | (HB) | |||
Standard Austenitic Stainless Steel |
NAS 301 |
SUS 301 |
≧205 | ≧520 | ≧40 | ≦90 | ≦200 | ≦187 |
NAS 304 |
SUS 304 |
≧205 | ≧520 | ≧40 | ≦90 | ≦200 | ≦187 | |
NAS 316 |
SUS 316 |
≧205 | ≧520 | ≧40 | ≦90 | ≦200 | ≦187 | |
Granular Corrosion |
NAS 301L |
SUS 301L |
≧215 | ≧550 | ≧45 | ≦95 | ≦218 | ≦207 |
NAS 304L |
SUS 304L |
≧175 | ≧480 | ≧40 | ≦90 | ≦200 | ≦187 | |
NAS 304LN |
SUS 304LN |
≧245 | ≧550 | ≧40 | ≦95 | ≦220 | ≦217 | |
NAS 316L |
SUS 316L |
≧175 | ≧480 | ≧40 | ≦90 | ≦200 | ≦187 | |
Duplex Stainless Steel | NAS 64 |
SUS 329J4L |
≧450 | ≧620 | ≧18 | HRC≦95 | ≦320 | ≦302 |
High Nickel |
NAS 155N |
- | ≧245 | ≧550 | ≧35 | ≦95 | ≦220 | ≦217 |
NAS 254N |
SUS 836L |
≧295 | ≧635 | ≧35 | ≦96 | ≦230 | ≦217 | |
NAS 354N |
- | ≧295 | ≧640 | ≧35 | ≦96 | ≦230 | - | |
Soft Austenitic Stainless Steel |
NAS 304MK |
SUS 304J2 |
≦155 | ≦600 | ≧55 | ≦80 | ≦155 | - |
NAS 304DJ |
SUS 304J1 |
≧175 | ≧480 | ≧40 | ≦90 | ≦200 | - | |
High Strength Stainless Steel |
NAS 631 |
SUS 631 |
≧380 | ≧1030 | ≧20 | ≦92 | ≦200 | ≦190 |
NAS 301N |
SUS 301 |
≧245 | ≧690 | ≧38 | ≦95 | ≦220 | - | |
Non-Magnetic |
NAS 305 |
SUS 305 |
≧175 | ≧480 | ≧40 | ≦90 | ≦200 | ≦187 |
NAS NM15M |
- | ≧390 | ≧690 | ≧30 | ≦98 | ≦228 | ≦240 | |
NAS 304LG |
- | ≧175 | ≧480 | ≧40 | ≦90 | ≦200 | ≦187 | |
NAS NM17 |
- | ≧175 | ≧480 | ≧40 | ≦90 | ≦200 | ≦187 | |
Oxidation Resistant |
NAS 302B |
SUS 302B |
≧205 | ≧520 | ≧40 | ≦95 | ≦218 | ≦207 |
NAS 310S |
SUS 310S |
≧205 | ≧520 | ≧40 | ≦90 | ≦200 | ≦187 | |
Ferritic Stainless Steel |
- | SUS 430 |
≧205 | ≧450 | ≧22 | ≦88 | ≦200 | ≦183 |
- | SUS 430LM |
≧175 | ≧360 | ≧22 | ≦88 | ≦200 | ≦183 |